Discrete model

Hamid Torabi's picture

Micromechanics of collective buckling in CNT turfs

Complex structures consisting of intertwined, nominally vertical carbon nanotubes (CNTs) are called turfs. Under uniform compression experiments, CNT turfs exhibit irreversible collective buckling of a layer preceded by reorientation of CNT segments. Experimentally observed independence of the buckling stress and the buckling wavelength on the turf width suggests the existence of an intrinsic material length.