Weixu Zhang's blog
Effect of surface stress on the asymmetric yield strength of nanowires
Submitted by Weixu Zhang on Wed, 2008-06-25 14:57.Effect of surface energy on the yield strength of nanoporous materials
Submitted by Weixu Zhang on Tue, 2006-12-19 01:55.This is a very rough manuscript but including the original material we used. Any criticism or suggestion is welcome. The only aim of this letter is to reflect the multi-effect of surface energy on material or structure in nanosize scale. Here we report the effect of surface energy on the yield strength of nanoporous materials. The conventional micromechanics method is extended to consider the surface effect and expression of effective yield surface of nanoporous materials in complex stress state is derived.
»