Synergism effect between nanofibrillation and interface tuning on the stiffness-toughness balance of rubber-toughened polymer nanocomposites: a multiscale analysis
Sat, 2023-05-13 05:09 - Mahdi Zeidi
In our recent study published in ACS Applied Materials & Interfaces, using a multiscale modeling technique, we investigated how the combination of nanofibrillation and interfacial tuning can have a synergistic effect on the stiffness-toughness balance in rubber-toughened nanocomposites. Check out the link below:
»