Improved oxidation resistance of high emissivity coatings on fibrous ceramic for reusable space systems
Thu, 2021-10-21 04:39 - Dr. Hanaor - De...
High emissivity coatings Radiate heat away from a reusable spacecraft while providing high temperature insulation during re-entry into Earth's atmosphere.
In this work the emissivity and stability of disilicide based coatings is studied. These materials exhibit intruiging self-healing properties and outstanding thermal performance.