Exploring the Low Cycle Fatigue Performance of FFF Steel 316L [Talk at AM Industry Summit]
[Talk at AM Industry Summit, 03 August 2021]
Exploring the Low Cycle Fatigue Performance of FFF Steel 316L
This talk, at the AM Industry Summit powered by ASME, will cover the findings from an ongoing investigation aiming to characterise the cyclic elastoplastic behaviour of fused filament fabricated (FFF) Steel 316L. The elastoplastic characteristics under stress and strain controlled loadings will be analysed for this material, in an attempt to understand the material's performance in low cycle fatigue (LCF) conditions.
Attendees will have the opportunity to learn how this popular fused filmanet fabrication (FFF) metal material performs under various cyclic loading histories. Practical considerations for the enhancement of the low cycle fatigue (LCF) performance will also be discussed.
Use code AMSPK199 to get one of the free passes
https://l.feathr.co/AMIndustry/August/2021/Speakers/Dr-Kyriakos-Kourousis
- kourousis's blog
- Log in or register to post comments
- 1441 reads
Recent comments