THis is the material data to be included in command file in ansys WB

 

 

 !********************

 

mpdele,all,matid

mpdata,KXX,matid,,0.192    

mpdata,C,matid,,1465 

UIMP,matid,REFT,,,22

mpdata,ALPX,matid,,8.3e-5 

mpdata,dens,matid,1170

TB,HYPE,matid,,2,MOON  

tbtemp,150

!TBDATA,,-.0456e6,.2331e6,0,,,

TBDATA,,-.0303e6,.4503e6,0,,,

TB,PRONY,matid,,10,SHEAR

!TBTEMP,0

TBDATA,,-4.10127,8.146128036,-2.21325,8.352182518,-0.74715,8.23299611,0.426511,7.956648579,1.439333,7.419955748,2.334454,6.931966115,3.396199,6.328379603,4.689309,5.824776462,6.287802,5.432969291,8.143015,5.008600172   

!TBDATA,1,-4.10127,2.146e6,-2.21325,2.35e6,-0.74715,2.232996e6,0.426511,1.956649e6,1.439333,1.419956e6,2.334454,0.931966e6,3.396199,0.32838e6,4.689309,-0.17522e6,6.287802,-0.56703e6,8.143015,-0.9914e6  

!TBDATA,,-4.10127,2.146,-2.21325,2.35,-0.74715,2.232996,0.426511,1.956649,1.439333,1.419956,2.334454,0.931966,3.396199,0.32838,4.689309,-0.17522,6.287802,-0.56703,8.143015,-0.9914  

!TBDATA,,0.00227236147414,2610.7,0.000594555311804,1872.5,1467.11042681,35602,5400.24327531,140.79,11690.6132846,3.2481    ! New calculated by curve fitting

!tbdata,,-2.64,3.416,-3.226,3.27,2.16,4.55,3.73,2.148,4.067,.5116   ! log of above row

!TB,PRONY,matid,,5,BULK 

!TBDATA,,0.16667,1,0.16667,1,0.16667,1,0.16667,1,0.16667,1   

TB,SHIFT,matid,,3,wlf

tbdata,190

!TBDATA,,109,16.14,56

TBDATA,,109,12,60

AttachmentSize
Image icon prony.jpg60.76 KB
Image icon mooney revlin constants.jpg105.06 KB
Image icon fig 1 Boundary cond.jpg177.12 KB
Taxonomy upgrade extras: 
Subscribe to Comments for "prony series"

Recent comments

More comments

Syndicate

Subscribe to Syndicate