A Theory of Ionic Polymer Conductor Network Composite

Ionic polymer conductor network composite (IPCNC) is a mixed conductor consisting of a network of loaded ionomer and another network of metallic particles. It is known that the microstructure of the composite, especially that of the electrodes, plays a dominating role in the performance of an IPCNC. However the microstructures of IPCNC have seldom been addressed in theoretical models. This letter formulates a continuum field theory for IPCNC by considering a supercapacitor-like microstructure with a large distributed interface area.