experimental mechanics; self-healing; zinc oxide; nanobelts; nanoindentation; dislocations
Electrical Self-Healing of Mechanically Damaged Zinc Oxide Nanobelts
Submitted by Xiaodong Li on Tue, 2011-12-27 18:55.We report the observation of remarkable electrical self-healing in mechanically damaged ZnO nanobelts. Nanoindentation into intrinsically defect-free ZnO nanobelts induces deformation and crack damage, causing a dramatic electrical signal decrease. Two self-healing regimes in the nanoindented ZnO nanobelts are revealed. The physical mechanism for the observed phenomena is analyzed in terms of the nanoindentation-induced dislocations, the short-range atomic diffusion in nanostructures, and the local heating of the dislocation zone in the electrical measurement. For details, please see
»
- Xiaodong Li's blog
- Login or register to post comments
- Read more
- 1378 reads


Recent comments
16 hours 12 min ago
21 hours 42 min ago
1 day 10 hours ago
2 days 11 hours ago
2 days 13 hours ago
2 days 13 hours ago
4 days 13 hours ago
4 days 16 hours ago
4 days 19 hours ago
4 days 22 hours ago