Effect of strain and oxygen vacancies on the structure of 180^o ferroelectric domain walls in PbTiO_3
Submitted by Arash_Yavari on Tue, 2010-01-05 20:49.In this paper, we study the effect of normal and shear strains and
oxygen vacancies on the structure of 180^o ferroelectric
domain walls in PbTiO_3.
»