TEM image showing uniformly distributed nano-fibers inside epoxy matrix
Submitted by Luoyu Roy Xu on Mon, 2007-02-26 20:43.
We observed that all nanofibers are curved not straight. So the Young’s modulus of the nanocomposite material is always lower than the model prediction using traditional micro-mechanics theory assuming straight nanofibers/nanotubes, as reported by Prof. Y. Huang’s group at UIUC.