Temperature dependence of the thermo-mechanical properties of aluminum
Submitted by omidomid on Thu, 2010-07-29 11:51.
I'm looking for the thermo-mechanical properties of aluminum, such as Young modulus, thermal expansion coefficient, thermal conductivity coefficient and poisson ratio as a function of temperature :
E=E0(1+E1*T+E2*T^2+E3*T^3) ; T: temperature in K
»
- omidomid's blog
- Login or register to post comments
- 2211 reads

Re: Temperature dependence of thermo-mechanical properties Al
See http://imechanica.org/node/1788 for specific heat, shear modulus and melting temperature. For other properties look at ASM Handbook-> Volume 2. Properties and Selection: Nonferrous Alloys -> Specific Alloys and Metal -> Properties of Wrought Aluminum->1050,1060,1145,1199,1350 (all have ~99.5 - 99.9 % Al).
-- Biswajit
While ASM Handbook is the
While ASM Handbook is the acceptable standard, you can also look at www.matweb.com for quick refernce . You will get all the properties of metal that you have mentioned. Most of the researchers in the simulation world use this website.
-Hardik
The Handbook of Aluminum,
The Handbook of Aluminum, Vol1. Physical Metallurgy and processes, edited by George E. Totten and D. Scott MacKenzie.
e_garcia
Temperature dependent elastic properties
You might also look at the data present in "Single Crystal Elastic Constants and Calculated Aggregate Properties. A Handbook" by Gene Simmons and Herbert Wang, MIT Press, 1971. You can fit your favorite curve to the data collected there.