A new finite element method for dislocations based on interior discontinuities
Comments and feedback of the following paper would be appreciated.
Abstract:
A new technique for the modelling of multiple dislocations based on introducing interior discontinuities is presented. In contrast to existing methods, the superposition of infinite domain solutions is avoided; interior discontinuities are specified on the dislocation slip surfaces and the resulting boundary value problem is solved by a finite element method. The accuracy of the proposed method is verified and its efficiency for multi-dislocation problems is illustrated. Bounded core energies are incorporated into the method through regularization of the discontinuities at their edges. Though the method is applied to edge dislocations here, its extension to other types of dislocations is straightforward.
| Attachment | Size |
|---|---|
| (2007 Gracie) A new fast finite element method for dislocations based on interior discontinuities.pdf | 1.76 MB |
- Robert Gracie's blog
- Login or register to post comments
- 2646 reads


Recent comments
4 hours 59 min ago
14 hours 37 min ago
15 hours 25 min ago
15 hours 54 min ago
16 hours 12 sec ago
22 hours 37 min ago
1 day 10 hours ago
1 day 11 hours ago
1 day 14 hours ago
2 days 8 hours ago