When a block of an elastomer is bent, the compressed surface may form a crease. This paper analyzes the critical condition for creasing by comparing the elastic energy in a creased body and that in a smooth body. This difference in energy is expressed by a scaling relation. Critical conditions for creasing are determined for elastomers subject to general loads and gels swelling under constraint. The theoretical results are compared with existing experimental observations.
»