Revision of Plastic deformation of freestanding thin films: Experiments and modeling from Thu, 2006-11-16 21:49
The revisions let you track differences between multiple versions of a post.
This is a paper we recently published in JMPS on a study of the mechanical properties on thin films comparing experimental results with discrete dislocation simulations. It provides insight in the strengthening that occurs in thin metal films when surface or interface effects become important.
The abstract is below; the full paper can be downloaded from here
Abstract - Experimental measurements and computational results for the evolution of plastic deformation in freestanding thin films are compared. In the experiments, the stress–strain response of two sets of Cu films is determined in the plane-strain bulge test. One set of samples consists of electroplated Cu films, while the other set is sputter-deposited. Unpassivated films, films passivated on one side and films passivated on both sides are considered. The calculations are carried out within a two-dimensional plane strain framework with the dislocations modeled as line singularities in an isotropic elastic solid. The film is modeled by a unit cell consisting of eight grains, each of which has three slip systems. The film is initially free of dislocations which then nucleate from a specified distribution of Frank–Read sources. The grain boundaries and any film-passivation layer interfaces are taken to be impenetrable to dislocations. Both the experiments and the computations show: (i) a flow strength for the passivated films that is greater than for the unpassivated films and (ii) hysteresis and a Bauschinger effect that increases with increasing pre-strain for passivated films, while for unpassivated films hysteresis and a Bauschinger effect are small or absent. Furthermore, the experimental measurements and computational results for the 0.2% offset yield strength stress, and the evolution of hysteresis and of the Bauschinger effect are in good quantitative agreement.
- Joost Vlassak's blog
- Login or register to post comments
- 6833 reads


Recent comments
32 min 18 sec ago
35 min 32 sec ago
3 hours 13 min ago
3 hours 49 min ago
4 hours 25 min ago
4 hours 46 min ago
5 hours 33 min ago
7 hours 12 min ago
7 hours 44 min ago
9 hours 15 min ago