Abstract:
Chip-packaging interaction is becoming a critical reliability issue for Cu/low k chips during assembly into a plastic flip-chip package. In a flip-chip package, the thermal deformation of the package can be directly coupled into the Cu/low k interconnect structure inducing large driving forces for interfacial crack formation. This chapter summarizes the experimental and modeling studies to investigate the chip-package interaction and its impact on low k interconnect reliability. First, the packaging induced deformation and stress at the chip level is analyzed using high-resolution moiré interferometry and compared to thermal and process-induced stresses during chip fabrication. Then, results from 3D finite element analysis (FEA) based on a multilevel sub-modeling approach to investigate the chip-package interaction for low k interconnects is presented. Packaging induced crack driving forces for relevant interfaces in Cu/low k structures are deduced and compared with corresponding interfaces in Cu/TEOS structures. Effects due to the solder, underfill and low k material properties on packaging reliability are examined. Finally, the effects of interconnect scaling and multilevel stacking on chip-package interaction and their impact on low k interconnect reliability is discussed.
Outline:
1. Introduction
2. Experimental Techniques
2.1 Thermal deformation of plastic flip-chip package
2.2 Measurement of interfacial fracture toughness
3. Mechanics of Cohesive and Interfacial Fracture in Thin Films
3.1 Channel cracking
3.2 Interfacial delamination
4. Modeling of Chip-Packaging Interactions
4.1. Multilevel sub-modeling technique
4.2 Modified virtual crack closure (MVCC) method
4.3 Package level deformation
4.4 Energy release rate for stand-alone chips
5. Energy Release Rate under Chip-Package Interactions
5.1 Effect of low k dielectrics
5.2 Effect of solder materials and die attach process
5.3 Effect of low k material properties
6. Effect of Interconnect Scaling and Ultra Low k Integration
7. Summary
Acknowledgments
References
| Attachment | Size |
|---|---|
| CPI_Review2007.pdf | 1.6 MB |
- Rui Huang's blog
- Login or register to post comments
- 1250 reads


Recent comments
1 hour 7 min ago
5 hours 9 min ago
5 hours 31 min ago
16 hours 14 min ago
16 hours 35 min ago
19 hours 39 min ago
1 day 4 hours ago
1 day 6 hours ago
1 day 6 hours ago
1 day 12 hours ago