You are here
Weyl Geometry and the Nonlinear Mechanics of Distributed Point Defects
Wed, 2012-07-25 09:00 - arash_yavari
In this paper we obtain the residual stress field of a nonlinear elastic solid with a spherically-symmetric distribution of point defects. To our best knowledge, this is the first nonlinear solution for point defects since the linear solution of Love in the 1920s.