Two modes of thin film buckling are commonly observed, one with interface delamination (e.g., telephone cord blistes) and the other with no delamination (i.e., wrinkling). Which one would occur for your films? This Letter gives a quantitative criterion for the selection of the buckling modes. An experiment was designed to show a transition of the buckling mode.
H. Mei, J.Y. Chung, H.-H. Yu, C.M. Stafford, and R. Huang, Buckling modes of elastic thin films on elastic substrates. Applied Physics Letters, to appear in April 2007.
| Attachment | Size |
|---|---|
| BW_transition v5.pdf | 134.2 KB |
»
- Rui Huang's blog
- Login or register to post comments
- 6335 reads


Recent comments
10 min 43 sec ago
47 min 21 sec ago
50 min 35 sec ago
3 hours 28 min ago
4 hours 4 min ago
4 hours 40 min ago
5 hours 1 min ago
5 hours 48 min ago
7 hours 27 min ago
7 hours 59 min ago