 <title>iMechanica - AISI 4150 or DIN 50CrMo4 Steel Flow Stress Curve Data for Machining Simulation - Comments</title>
 <link>http://www.imechanica.org/node/7844</link>
 <description>Comments for &quot;AISI 4150 or DIN 50CrMo4 Steel Flow Stress Curve Data for Machining Simulation&quot;</description>
 <language>en</language>
<item>
 <title>hie</title>
 <link>http://www.imechanica.org/node/7844#comment-13987</link>
 <description>&lt;p&gt;I am also looking for the stress starin curves of related material 51CrMoV4 .....(AISI 4150) ..for details go to my blog :&amp;nbsp;&lt;/p&gt;
&lt;p&gt;&amp;nbsp;&lt;span class=&quot;Apple-style-span&quot;&gt;&lt;a href=&quot;http://imechanica.org/node/7870&quot;&gt;Flow Stress Curves for 51CrMoV4 material at varying temperature and strain rates&lt;/a&gt;&lt;/span&gt;&lt;/p&gt;
&lt;p&gt;cheers,&lt;/p&gt;
&lt;p&gt;Krunal.&amp;nbsp;&lt;/p&gt;
&lt;br class=&quot;clear&quot; /&gt;</description>
 <pubDate>Sat, 27 Mar 2010 08:03:57 -0400</pubDate>
 <dc:creator>kruzster</dc:creator>
 <guid isPermaLink="false">comment 13987 at http://www.imechanica.org</guid>
</item>
<item>
 <title>Thank you very much for the</title>
 <link>http://www.imechanica.org/node/7844#comment-13944</link>
 <description>&lt;p&gt;Thank you very much for the reference. But 4150 has 10percent lesser reduction in area % and 2 percenl lesser elongation when compared to 4340 and so the material model will definitely change because of this. I am still searching for the material model. So if you come across, the material model somewhere, please let me know. Thank you very much.&lt;/p&gt;
&lt;p&gt;With Best Regards&lt;/p&gt;
&lt;p&gt;Ashwin Devotta&lt;/p&gt;
&lt;p&gt;&lt;a href=&quot;mailto:ashwin.devotta@gmail.com&quot;&gt;ashwin.devotta@gmail.com&lt;/a&gt;&lt;/p&gt;
&lt;p&gt;&amp;nbsp;&lt;/p&gt;
&lt;br class=&quot;clear&quot; /&gt;</description>
 <pubDate>Tue, 23 Mar 2010 02:34:07 -0400</pubDate>
 <dc:creator>ashwin.devotta</dc:creator>
 <guid isPermaLink="false">comment 13944 at http://www.imechanica.org</guid>
</item>
<item>
 <title>Re: AISI 4150 flow stress data</title>
 <link>http://www.imechanica.org/node/7844#comment-13925</link>
 <description>&lt;p&gt;
If 4150 and 4340 have similar compositions you should be able to use the flow stress data from 4340 that you can find on my paper linked to on&lt;a href=&quot;http://imechanica.org/node/1278&quot;&gt; http://imechanica.org/node/1278&lt;/a&gt;.
&lt;/p&gt;
&lt;p&gt;
The flow stresses are similar for many steels even though the strains to failure may be quite different.
&lt;/p&gt;
&lt;p&gt;
-- Biswajit
&lt;/p&gt;
&lt;br class=&quot;clear&quot; /&gt;</description>
 <pubDate>Sun, 21 Mar 2010 23:30:09 -0400</pubDate>
 <dc:creator>Biswajit Banerjee</dc:creator>
 <guid isPermaLink="false">comment 13925 at http://www.imechanica.org</guid>
</item>
<item>
 <title>AISI 4150 or DIN 50CrMo4 Steel Flow Stress Curve Data for Machining Simulation</title>
 <link>http://www.imechanica.org/node/7844</link>
 <description>&lt;p&gt;Hi All,&lt;/p&gt;
&lt;p&gt;I am into machining simulation of 50CrMo4 Steel in DEFORM 3D and I need the flow stress curve data for various temperature and various strain rates. I have searched in as many journals as possible, but in vain. It would be of immense help if some one could share the material model data with me.&lt;/p&gt;
&lt;p&gt;Thanking you in advance&lt;/p&gt;
&lt;p&gt;With Best Regards&lt;/p&gt;
&lt;p&gt;Ashwin Devotta&lt;/p&gt;
&lt;p&gt;ashwin.devotta@gmail.com&amp;nbsp;&lt;/p&gt;
&lt;br class=&quot;clear&quot; /&gt;</description>
 <comments>http://www.imechanica.org/node/7844#comments</comments>
 <category domain="http://www.imechanica.org/taxonomy/term/390">Materials Forum</category>
 <category domain="http://www.imechanica.org/taxonomy/term/962">software</category>
 <category domain="http://www.imechanica.org/taxonomy/term/4954">AISI 4150 Steel</category>
 <category domain="http://www.imechanica.org/taxonomy/term/4955">DIN 50CrMo4 Steel</category>
 <category domain="http://www.imechanica.org/taxonomy/term/4953">flow stress curve</category>
 <category domain="http://www.imechanica.org/taxonomy/term/4956">Johnson Cook Model</category>
 <category domain="http://www.imechanica.org/taxonomy/term/4952">Machining simulation</category>
 <pubDate>Sun, 21 Mar 2010 17:53:30 -0400</pubDate>
 <dc:creator>ashwin.devotta</dc:creator>
 <guid isPermaLink="false">7844 at http://www.imechanica.org</guid>