Study on electroelastic field concentration around the electrode tip in multilayer ferroelectric actuators
Submitted by Xujun Zhao on Sat, 2010-09-11 15:20.Distribution of electromechanical field near electrode tips is closely related to the reliability of ferroelectric multilayer actuators. In this paper, the deformation and stress concentrations around the electrode tip in two multilayer actuator designs, partially and fully cofired, are investigated by means of experimental measurement and numerical simulations. The digital speckle correlation method (DSCM) is used to measure the full displacement field near the electrode tip with the high spatial resolution. The paths of electric breakdown and cracks initiated from the edge of electrodes were observed.