EM 397 Term Paper: Effects of Substrate Compliance on Buckling Delamination of Thin Films under Compression
Submitted by Haixia Mei on Wed, 2006-11-29 18:12.For films or coatings deposited on substrate at high temperature, residual compressive stresses are often induced in the surface layers because of the mismatch in the thermal expansion coefficients. Under such compressive residual stresses, the surface thin film is susceptible to buckling-driven delamination. Various shapes of buckled region are observed, including long straight-sided blisters, circular and the ‘telephone cord’ blister.
»