Submitted by Xi Wang on Sun, 2009-02-01 23:16.Laser Annealing of Amorphous NiTi Shape Memory Alloy Thin Films to Locally Induce Shape Memory Properties
Submitted by Xi Wang on Sat, 2006-11-04 05:32.Xi Wang, Yves Bellouard, Joost J. Vlassak
Published in Acta Materialia 53 (2005) p4955-4961.
Abstract — We present the results of a crystallization study on NiTi shape memory thin films in which amorphous films are annealed by a scanning laser. This technique has the advantage that shape memory properties can be spatially distributed as required by the application. A kinetics study shows that nucleation of the crystalline phase occurs homogenously in the films. Consequently, the laser annealing process produces polycrystalline films with a random crystallographic texture. The crystallized films have a uniform microstructure across the annealed areas. The material in the crystalline regions transforms reversibly to martensite on cooling from elevated temperature and stress measurements show that a significant recovery stress is achieved in the films upon transformation.
- 1 comment
- 90815 reads


Recent comments
1 hour 19 min ago
4 hours 55 min ago
9 hours 4 min ago
9 hours 30 min ago
12 hours 39 min ago
12 hours 55 min ago
12 hours 59 min ago
13 hours 28 sec ago
13 hours 31 min ago
13 hours 43 min ago